A novel synthesis route of Eu2+-doped pure-nitride α-sialons has been reported. It is through an alloy-nitridation method at ∼2173K in nitrogen atmosphere, with stable alloys (CaAl, SiEu), AlN, and α-Si3N4 powders as starting materials. A linear relationship between the lattice parameters and m values of (Ca0.995Eu0.005)m/2Si12−mAlmN16 compositions is obtained, indicating that our samples contain very little oxygen, i.e. herein so-called Eu-doped pure-nitride α-sialons. The (Ca0.995Eu0.005)m/2Si12−mAlmN16 compounds with 2.4≤m≤4.0 give the strongest emission. The emission shifts to longer wavelength with m values increasing as well as Eu contents increasing. (Ca0.995Eu0.005)m/2Si12−mAlmN16 compositions with smaller m values exhibit better thermal quenching properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.