Abstract

Zinc leaching residue is a good source of zinc and has a great potential to be utilized. However, it is very difficult to recover lead, zinc and silver from the residue by traditional technologies. In this study, a new technology based on conversions of PbSO4 and ZnSO4 in the residue to their respective sulfides by reduction roasting with coal powder followed by a flotation treatment was developed. The effects of roasting temperature, coal dosage, reaction time and pyrite dosage were investigated at a laboratory scale. The results showed that the conversion extent of PbSO4 and ZnSO4 under the optimal experimental conditions was 71.89 and 69.76%, respectively. A flotation concentrate containing 39.13% Zn, 6.93% Pb and 973.54 g/Mg Ag was obtained from the treated material, and the recovery of Zn, Pb and Ag was 48.38, 68.23 and 77.41%, respectively. The tailing containing ZnFe2O4 or Fe3O4 could be either stockpiled or further disposed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.