The corrosive erosion behavior of Ti–51at.%Ni alloy under different erosion conditions was studied and compared to that of 304 stainless steel. Erosion tests were performed in a slurry-pot tester with dry sand, 3.5% NaCl slurry and 0.1 mol l −1 H 2SO 4 slurry containing 30% silica sand, respectively. Synergistic effects of corrosion and erosion were studied in steady corrosion, polarization, dry sand errosion and micro-wear experiments. An electrochemical-scratching test characterized the failure and recovery of the passive film formed on TiNi alloy in 3.5% NaCl and 0.1 mol l −1 H 2SO 4 solutions, respectively. In both dry sand and the corrosive media, the TiNi alloy exhibited considerably greater erosion resistance than 304 stainless steel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.