Abstract

This paper is focused on the experimental research of Fe-based oxygen carriers using coal ash as support material. Influence of coal ash size, foamer content, temperature on reactivity of Fe-based oxygen carrier for CO oxidation were conducted in thermogravimetry analyzer (TGA). Experimental results show that conversion of the oxygen carrier could attain 100% under 750 °C, and samples that made from mean coal ash grain size of 0.06 mm are more active than that of 0.09 mm, which prove tiny coal ash grain size can enhance reactivity of oxygen carriers. Besides, reactivity of oxygen carriers under 850 °C are lower than 750 °C for that relative high temperature would cause sintering of the Fe-based oxygen carriers.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.