Abstract

The bonding of orthodontic brackets to enamel is a multistep process. To simplify bonding and decrease chair time, Transbond Plus Self-Etching Primer (3M Unitek, Monrovia, Calif) has been introduced; the primer combines the etching, rinsing, and priming steps. This in vitro study evaluated the shear bond strengths and interoperator variability of self-etching primer, as compared with conventional phosphoric acid etching with 2 common orthodontic resins. A total of 214 teeth were bonded, according to the following protocols: group A: self-etching primer plus Transbond XT light-cured resin (3M Unitek); group B: 35% phosphoric acid (15 seconds) plus Transbond XT resin; and group C: 37% phosphoric acid (15 seconds) plus Enlight bonding resin (Ormco, Glendora, Calif). Significantly higher bond strengths were seen in group B than in group A ( P = .004) and group C ( P = .002). The mean shear bond strengths of group A were not significantly different from those of group C ( P = .99). When 3 orthodontists bonded a total of 60 premolars using the protocols of groups A and B, significant differences in shear bond strengths and strength ranking were found. The mean values they obtained using the self-etching primer were not significantly different, but significant differences in mean values were found between operators when the phosphoric acid-etching technique was used.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.