AbstractClose‐packed arrays of Au nanoparticles are produced in patterned regions by electron beam (e‐beam) lithography using a highly sensitive direct–write resist, N+AuCl4−(C8H17)4Br. While the e–beam causes dewetting of the resist to nucleate Au nanoparticles, the following step of thermolysis aids particle growth and removal of the organic part. Thus formed arrays contain Au nanoparticles. Such arrays are patterned into ≈10 μm wide stripes between Au contact pads on SiO2/Si substrates to realize electrical rectification. Under forward bias, the device exhibits a threshold voltage of +4.3 V and a high current rectification ratio of 3 × 105, which are stable over many repetitive measurements. The threshold voltage of the rectifier can be reduced by applying an electric stress or by varying the electron dosage used for array formation. The nanoparticle rectifier element could be transferred onto flexible substrates such as PDMS, where the nanoparticle coupling is influenced by swelling of the substrate. Obviously, the nanoparticle size, shape, and the spacing in array are all important for the rectifier device performance. Based on the electrical measurements the mechanism of rectification is found to be due to switching of electrical conduction with applied bias, from short–distance tunneling to F–N type tunneling followed by transient filament formation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.