Abstract
AbstractA new method for identification of ethylene/α‐olefin copolymer was established by Fourier Transform Infared (FTIR)–Differential Scanning Calorimetery (DSC) in this article. DSC and FTIR spectroscopy techniques were used to analysis the type and content of α‐olefin in polyolefine copolymer. FTIR was available to identify the structures of polyethylene and copolymers of ethylene with different α‐olefins. The type of polyethylene can be determined by the peak position of 1378 and 1369 cm−1. According to the peak location of 770, 784, and 895 cm−1, the type of α‐olefin can also be determined. DSC method was used to decide the position of melting peaks. The quantitative investigation of the content of α‐olefin in polyethylene was calculated by the formula: −ln(CH2 mol fraction) = −0.331+135.5/Tm. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.