Abstract
In this paper, we describe an automatic detection system to recognise welding defects in radiographic images. In a first stage, image processing techniques, including noise reduction, contrast enhancement, thresholding and labelling, were implemented to help in the recognition of weld regions and the detection of weld defects. In a second stage, a set of geometrical features which characterise the defect shape and orientation was proposed and extracted between defect candidates. In a third stage, an artificial neural network (ANN) for weld defect classification was used. With the aim of obtaining the best performance of ANN three different methods for improving network generalisation was used. The results was compared with a method without generalisation. For the input layer, the principal component analysis technique was used in order to reduce the number of feature variables; and, for the hidden layer, a different number of neurons was used.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.