Abstract
A kind of slurry which is applicable for fine atomizing CMP was made and the optimal results were obtained through orthogonal experiments by comparing fine atomizing CMP and traditional CMP. The research results show that the material removal rate of fine atomizing CMP is 52.23% of traditional CMP, and the dosage of the slurry used in fine atomizing CMP only accounts for 10 vol% compared to traditional CMP. The surface roughness after the fine atomizing CMP is 2.5nm which is better than that of the traditional CMP (3.0nm).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.