Abstract
An acoustic emission study of stress corrosion cracking in GFRP : 40519 Hill, R.; Cowking, A.; Carswell, W.S. Proceedings of the 16th European Working Group on Acoustic Emission Conference, London (United Kingdom), 13–18 Sep. 1987, pp. 2872–2880. Edited by C.B. Scruby and R. Hill, Proceedings of the 4th European Conference on Non-Destructive Testing, London (United Kingdom), 13–17 Sep. 1987, Vol.