Abstract

The forming process of drawing texture and the recrystallization behavior of (α+β) brass rod have been investigated by means of determination of the ODF and transmission electron microscopy.The preferred fiber component is composed of the 〈111〉+〈100〉 duplex fiber texture which is less in intensity than that of α mono-phase brass rod because of the presence of β-phase. The fiber component in β-phase is composed of the 〈110〉 fiber texture which is a stable orientation in bcc metals. The volume fraction of β-phase increases with the increase of the drawing ratio and reaches about 40% by drawing to 90% reduction, because the distorted β′-phase and fct α1-phase are developed during deformation.Regarding the recrystallization behavior, the 〈111〉 fiber texture remains in α-phase, and the 〈110〉 fiber texture remains in β-phase with the continuous recrystallization.Microscopic examination shows that the α-phase bulges into the β-phase on annealing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.