Al-matrix SiC whisker composites were fabricated by pressureless infiltration of liquid Al-Mg or Al-Si-Mg alloys at 830–950°C in the presence of N2 into a preform of nickel coated SiC whiskers. The nickel coating on the whiskers was obtained by electroless plating and made pressureless infiltration possible. The composite made by pressureless infiltration exhibited slightly lower tensile strength and modulus and slightly higher coefficient of thermal expansion than the corresponding composite made by pressure infiltration. However, the differences were small in spite of the lack of prior evacuation in the pressureless infiltration case. On the other hand, the hardness decreased with increasing distance from the preform-melt interface much more significantly in composites made by pressureless infiltration than those made by pressure infiltration. The hardness decrease, which was attributed to a porosity increase, was larger for composites made by pressureless infiltration without prior evacuation than those made by pressureless infiltration with prior evacuation. The Al-SiC reactivity was larger for composites made by pressureless infiltration than those made by pressure infiltration, because the infiltration time was longer in pressureless infiltration.[/p]

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.