Abstract

The coking resistance of six alumina supported nickel catalysts in n-butane steam reforming mainly depends on the average size of nickel crystallites. Thus, by using suitable preparative methods, it is possible to produce good, coking resistant nickel catalysts even with Al2O3 support.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.