Abstract
Abstract.A device design is proposed that makes it possible to obtain composite castings of sliding bearings based on babbitt by mixing alloying additives from antifriction powders of solid lubricants (graphite, molybdenum disulfide, etc.) into the melt, having a density significantly lower than the density of babbitt itself. The principle of mixing is based on the use of numerous turbulent flows resulting from the rotation of a gating rod with a wire pile in the melt material, the packing density coefficient of which is not less than 0.1. Due to the suction effect of these flows, non-metallic particles of solid lubricant powder do not float to the surface of the melt and, after crystallization, remain in the body of the casting. The supply of alloying powder of solid lubricant is carried out simultaneously with the supply of the babbitt melt through the central and distribution gating channels made in a rotating rod. Under the action of centrifugal forces, powder particles and melt material flow through distribution channels to the walls of the mold (mold), passing through the rotation zone of the metal pile. In this case, intensive mixing of the powder particles with the melt material occurs due to the suction effect of turbulent flows arising behind the moving pile. In addition, as a result of the rotation of the wire pile, dendritic constituents are crushed in babbitt castings. Metallographic studies of the castings obtained on the developed device have shown that the structure of the casting obtained by traditional technology contains large quantities of solid crystals of intermetallic compounds SnSb and Cu3Sn, while in the structure of the casting obtained using the proposed device, along with the aforementioned intermetallic compounds, particles of solid lubricant C + MoS2powder embedded in the crystallized melt are observed.
Highlights
A device design is proposed that makes it possible to obtain composite castings of sliding bearings based on babbitt by mixing alloying additives from antifriction powders of solid lubricants into the melt, having a density significantly lower than the density of babbitt itself
Turbulent flows resulting from the rotation of a gating rod with a wire pile in the melt material, the packing density coefficient of which is not less than 0.1
Due to the suction effect of these flows, non-metallic particles of solid lubricant powder do not float to the surface of the melt and, after crystallization, remain in the body of the casting
Summary
A device design is proposed that makes it possible to obtain composite castings of sliding bearings based on babbitt by mixing alloying additives from antifriction powders of solid lubricants (graphite, molybdenum disulfide, etc.) into the melt, having a density significantly lower than the density of babbitt itself. Республика Беларусь Тел.: +375 17 292-74-54 metech@bntu.by Перспективным направлением улучшения работоспособности подшипников скольжения на основе баббита является применение модифицированных композиционных баббитовых материалов, получаемых либо путем спекания порошковых смесей баббита с наноразмерной алмазнографитной шихтой УДАГ [2], либо посредством литья с введением в расплав легирующих добавок из компонентов твердой смазки (графита, дисульфида молибдена, углеродных нанотрубок и др.) [3, 4].
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.