Abstract

The changes in morphology and crystalline state of solution-grown single crystals of poly(L-lactic acid)(PLLA) in aqueous NaOH solution of various strengths were investigated by means of transmission electron microscopy, atomic force microscopy and gel permeation chromatography. The degradations of hexagonal and lozenge shaped PLLA single crystals started from the lateral side of the crystal to generate the notched morphology at initial stage of hydrolysis. As hydrolysis proceeded, the molecular weight of degraded PLLA crystals corresponded to equal the value calculated from lamellar thickness measured by atomic force microscopy, suggesting that the tight chain-folding region of PLLA molecules on crystal surface was degraded by alkaline hydrolysis. Based on the results, alkaline hydrolysis with NaOH solution firstly occurs at the loosely chain-packing region on crystal edges, and then gradually progresses from both crystal edges and tight chain-packing region with chain-folding on the crystal surface.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.