Abstract

The technology of obtaining a coagulant—aluminum hydroxychloride—from aluminum chip by the alkali-acidic method is investigated. In this method, the largest part of impurities present in the starting raw material is separated during the filtration of the aluminate solution. The reagent for the removal of oils, petroleum derivatives, and lubricoolant from the surface of aluminum chip is selected. A new principal process flow chart for obtaining the coagulant by the alkali-acidic method is suggested. The flow chart allows one to obtain a coagulant with a minimal content of impurities with the simultaneous liberation of chlorine for water disinfection and sodium hydroxide for the alkali dissolution of aluminum chip.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.