Abstract Co–MnO catalysts have been prepared by pyrolytic decomposition of the corresponding fumarate or gluconate salts and examined in the reactions of methanol and ethanol reforming. The synthesis parameters were the type of organic salt, the Co:Mn ratio and the temperature of decomposition. The decomposition pathway depends on the type of carboxylate, with the fumarate group being more stable than the gluconate. In-situ XRD measurements of salt decomposition showed that the reducing atmosphere prevailing during thermal treatment, as well as the presence of solid carbon, facilitates reduction of cobalt oxides towards metallic cobalt at temperatures above ∼500 °C. Thus, the reduced form of the catalyst, consisting mainly of metallic cobalt and MnO dispersed in a carbonaceous matrix can be prepared in a single step. It was found that reforming of both methanol and ethanol proceeds under comparable reaction conditions and hydrogen yield is maximized at temperatures of 400–450 °C. The activity of catalysts prepared under an inert atmosphere was considerably higher than the one of catalysts prepared through oxidative pre-treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.