Abstract

Abstract Alcohol oxidase was covalently immobilized onto magnetic beads of two different sizes, 75–150 μm and 50–75 μm in diameter, fabricated in the presence of glycidylmethacrylate and methylmethacrylate via suspension polymerization in the presence of a cross-linker (i.e., ethylenedimethylmethacrylate). The activity of the enzyme on smaller microspheres was found to be almost 4.8 fold higher than that of the larger counterparts. Although enzyme loading was same for both fractions, activity and the affinity of immobilized enzyme were significantly altered. The effects of various parameters such as temperature, pH, operational and storage stability were examined. The substantial change in the activity of enzyme was also observed in stability experiments in favor of large size magnetic beads. For all stability experiments including storage stability, the 75–150 μm fraction was found to be more sentinel support for the enzyme.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.