Abstract

It is pointed out that the magnetic material for cores of a differential current transformer (DCT) of a ground fault interrupter (GFI) should be characterized by high initial permeability, little dependence on temperature, and a low remanence. These parameters have been taken into consideration during selection of the most suitable annealing regime of Co-based (CoFeMnMo)/sub 77/(SiB)/sub 23/ material. It is assumed that a GFI is required to have a service life of 20-years continuous operation. Hence, the magnetic properties of the core of the DCT must be highly stable and exhibit virtually no deterioration over this period. During its operational lifetime, the core may be subjected to rapid saturation due to short circuits and earth faults, etc., as well as cyclic temperature changes. The effects of temperature aging and high current transients on the performance of the DCT were investigated. It is concluded that current shocks do not significantly alter the small-signal magnetic permeability of Co-based amorphous cores of selected annealing. The material examined exhibits degradation of magnetic properties due to aging greater than that reported for Fe-based materials.< <ETX xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">&gt;</ETX>

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.