Abstract

Accelerated aging of spruce wood samples have been carried out by thermo-hydro (TH) treatments. These treatments were applied to accelerate the chemical reactions that take place during the natural aging of wood. In order to avoid dissimilar chemical reactions between the TH treatments and the natural aging, mild temperatures (between 100 and 150°C) have been selected at low relative humidity (RH). The mechanical properties of non-aged, natural aged and accelerated aged spruce wood have been compared. It is apparent that longitudinal Young's modulus of accelerated aged wood increase slightly at the beginning of the treatment and is followed by a reduction. Along the radial direction, Young's modulus remains almost unchanged. On the other hand the radial strength is severely reduced. From these results, the relative radial strength has been fitted on the chemical kinetic law. The rate constant of this law has been calculated and the treatment temperature and wood moisture content have been integrated. Finally this law has been extrapolated to standard climatic conditions in order to predict the loss of strength of old wood by knowing its age and its mean climate history of temperature and RH (ambiance condition).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.