Abstract
The SHS process of the Ti-Cr-Al-C powder mixture is studied in the paper. The increase in the content of chromium in the mixture is shown to decrease the maximum temperature of the front of combustion wave. If the content of chromium in the mixture is above 20 wt.%, the process proceeds in the nonstationary combustion mode. Nanolaminate phases Ti2AlC and Ti3AlC2 or their mixtures are found to be formed when the content of chromium is not more than 20 wt. %. The addition of chromium increases the oxidation resistance of materials which can be recommended for use under extreme operating conditions, as an example for electrical contacts, bearings, heating elements, heat exchangers, and high-temperature ceramics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.