Abstract

The paper presented the mechanical (MChT), microwave (MWT), and hydrothermal (HTT) methods of zirconium phosphate samples modification in order to improve its adsorption affinity for the Ag (I) ions. The FTIR studies proved that the modification of both gel and xerogel samples with the ultrasonic microwaves causes an increase in the concentration of phosphate groups on the surface of MWT-modified zirconium phosphate: the isoelectric point pHiep = 2.2–2.9 for these samples against 3.9 for the initial sample and pKa2 values were 4.7–5.6 and 6.3, respectively. As resulting from the Ag+ ion adsorption studies, the MWT treatment of zirconium phosphate samples caused the greatest affinity of Ag+ ions for the surface of MWT zirconium phosphate. Compared with the initial ZrP sample, the shift of the Ag (I) ion adsorption edge towards lower pH values was observed, e.g., with adsorption of Ag (I) ions from the solution with the initial concentration of 1 µmol/dm3 for the initial ZrP sample pH50% = 3.2, while for the sample MWT ZrPxero pH50% = 2.6.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.