Introduction: The conditioning procedures for glass-based ceramic restorations before adhesive cementation are generally recognized. In the case of polycrystalline ceramics, which include zirconium oxide, there is still no standardized protocol. The aim of this work was to present conditioning methods of the cementation surface of zirconium oxide fixed dentures. The new generation high translucency zirconia has been also considered. Material and method: The following keywords for the PUBMED and EMBASE databases were used: zirconium oxide, zirconium oxide with increased translucency, bond strength, bending strength, surface treatment. The inclusion criteria were original papers in English published between 2015–2021. Results: Out of 1537 publications, 53 articles were selected for the study, covering methods of conditioning zirconium ceramics, including new materials with increased translucency. These procedures were divided into 5 main groups. Summary: Due to the widespread use of zirconia ceramics and the introduction of new zirconia-based materials, the use of a predictable and standardized cementation protocol is one of the most important factors contributing to the long-term clinical success of prosthetic restorations. Therefore, the research showed differences in the properties of the covered materials after conditioning. It suggests the need to create separate conditioning protocols for highly translucent and traditional zirconia.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.