Abstract

The effect of physical (ultrasonic) and chemical (exposure in 3% solution of acetic acid) activation of filler on the adhesion strength of the protective coatings based on styrene–acrylic dispersions to different substrates is studied. It is shown that modification of kaolins allows one to increase the adhesion strength by 40–50% in the case of the physical activation and by 1.1–1.2 times in the case of chemical activation. The best results are achieved with the use of E-21 dispersion as the polymer matrix.