Bioactive TiO(2) coatings have been found to enhance fibroblast adhesion and gingival attachment on the titanium surfaces, but no information is available whether the coatings also promote the adhesion of periodontal pathogens. The purpose of this study was to investigate protein adsorption and the adhesion of Aggregatibacter actinomycetemcomitans (Aa) and Fusobacterium nucleatum (Fn) on bioactive TiO2 surfaces. Commercially pure titanium discs (diameter 11.0 mm, grade 2) were coated with sol-gel derived bioactive TiO2 coatings (MetAlive, Vivoxid, Turku, Finland) and preincubated in 1.5 ml PBS/diluted serum/diluted saliva at room temperature to mimic the clinical situation after implantation and to allow serum/saliva proteins to adhere on the substrates. Uncoated titanium discs were used as controls. SDS-PAGE revealed similar protein profiles on bioactive and control titanium substrates. No differences were noticed in Aa or Fn adhesion between bioactive and control titanium. However, serum and saliva conditioning diminished Aa adhesion on both surfaces (p<0.001). It can be concluded that bioactive TiO2 coating does not promote adhesion of Aa and Fn.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.