ObjectivesBond durability and resistance to acid-base challenge of dentin with dual-cure resin cement have been rarely investigated. The purpose of this study was to evaluate dentin bond strength and observe the adhesive-dentin interface after acid-base challenge using three different dual-cure resin cements. MethodsThirty dentin surfaces from caries-free human premolars were ground and bonded with one of three dual-cure resin cements: PANAVIA V5 (V5), ESTECEM II (E II) and Rely X Ultimate (RXU) and thermocycled for 0, 5,000 and 10,000 cycles. A microtensile bond strength (μTBS) test was undertaken and the interface of the bonded specimens after acid-base challenge was examined by SEM. ResultsThe μTBS of V5 exhibited a stable bond strength despite thermal cycling while the bond of EII and RXU after 10,000 cycles dropped significantly among all thermal cycle periods (p<0.05). An acid-base resistant zone (ABRZ) was observed in all groups, however, the morphology of the bonded interface differed among the tested cements. ConclusionBonding durability to dentin and ABRZ morphologies differed among the cements evaluated. PANAVIA V5 cement system with tooth primer provided the most reliable bond strength and was best able to resist the acid–base challenge.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.