Abstract

This study aimed to evaluate the interface of universal adhesive (UA) with bulk-fill resin (BF) and dentin, after endodontic irrigation. The pulp chamber of 96 molars was irrigated with chlorhexidine 2% (CHX) or sodium hypochlorite 5.25% (NaOCl) and restored according to three restorative protocols. Microtensile bond strength (μTBS) and nanoleakage tests were performed after 24 h of thermocycling. Kruskal Wallis, Mann-Whitney and Wilcoxon were performed (p < 0.05). Comparing restorative systems, a difference was found only when irrigated with CHX after 24 h. CHX provided higher μTBS than NaOCl after 24 h for two restorative protocols; after thermocycling, NaOCl provided the greatest μTBS than CHX for one group. Decreased μTBS was observed for all restorative systems when CHX was used after thermocycling. NaOCl demonstrated the highest nanoleakage. The composition of UA influenced the immediate adhesion and sealing to BF when CHX was used; ageing has a deteriorating effect on adhesion and sealing for all restorative systems.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.