Multi-materials were designed for the severe corrosion environment in fluorine chemical industry. Directed energy deposition with laser beam (DED-LB) was used to manufacture SS316L/IN625 multi-materials with direct combination (DC) and graded transition (GT) structures. Partial immersion tests in 40% HF solution were conducted. The corrosion rate of SS316L/IN625 multi-materials was less than 1 mm/y. However, localized galvanic corrosion was observed in the DC samples because of the sudden change in chemical composition at the interface. The GT samples effectively eliminated this issue by gradually increasing Ni, showing good economic efficiency and reliability for the multi-phase HF corrosion environment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.