Abstract
The equilibrium experiments between CaO-Al2O3-MgO-0.06 to 0.85%MnO-0.5 to 2.1%FetO-0.07 to 0.3%S (mass content in %) slag and liquid iron were carried out at 1823 and 1873 K in order to assess the activities of Al2O3 and MgO along the spinel (MgO·Al2O3) saturation line. The activities of CaO in an entire liquid region were first determined at 1823 and 1873 K from the reported values for sulfide capacity, coupled with the activity coefficients of CaS which were estimated from those in the CaO-Al2O3 slags. On the basis of these iso-activity lines for CaO, the activities of Al2O3 and MgO were calculated by using he method of Schuhmann, in which the assessed activities of Al2O3 and MgO on the spinel saturation line were taken as the starting points. The activity coefficients of FetO and MnO along the spinel saturation line were determined and the deoxidation equilibria of Al, Mg, and Ca were discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.