Abstract

In view of the LHC upgrade for the High Luminosity phase (HL-LHC), the ATLAS experiment plans to replace the Inner Detector with an all-silicon system. The n-on-p silicon technology is a promising candidate to achieve a large area instrumented with pixel sensors, since it is radiation hard and cost effective. The paper reports on the performance of thin 100 and 130 μ m n-in-p planar pixel sensors produced by FBK-CMM with active-edge technology in collaboration with LPNHE and INFN. Beam-test results are presented, with focus on the hit efficiency at the detector edge of a novel design consisting of a staggered deep trench.