Abstract

The literature reports values ranging from 8000 to 26,000 cal per g-atom for the activation energy for the creep of tin. The present investigation analyzed the results of constant stress creep tests during steady state creep, and by means of temperature cycling. A value of approximately 9000 cal per g-atom for the creep of high purity tin in the temperature range 300 to 350° K was obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.