Abstract

Graphite oxide was prepared by acidification assisted Hummers method, which contains acidification, medium temperature and high-temperature three stages. Traditional Hummers low-temperature process was replaced by acidification process. The dosages of acid, graphite and potassium permanganate were investigated, and the produced graphite oxide was treated by ultrasonic oscillation and reduced to graphene by refluxing the reaction mixture at 100°C under open-air conditions. The structure of natural graphite, graphite oxide and graphene were characterized by X-ray diffractometry and infrared spectrum, the morphology of graphene was observed on a scanning electron microscope and the electrochemical properties of graphene were analyzed by the three-electrode cyclic voltammetry test system.