The grade of final celestite concentrate is as high as 95–96% after jigging and table washing operations applied by Barit Maden Turk in Turkey. Celestite concentrate contains 95% SrSO 4, and 3% CaSO 4, 0.5%BaSO 4, 0.5% SiO 2, 0.5%Fe 2O 3 as major impurities. Before the conversion of celestite to strontium carbonate with the double decomposition method, the iron content of celestite must be decreased to below 0.10 g/L. This study concerns the acid leaching of Turkish celestite concentrate. A purity of celestite of 98% could be obtained using 50% H 2SO 4 and 1–3% HNO 3 at 40–50 °C and the content of the impurities is about 0.005% Fe, 0.11% Ca, 0.6% Ba, 0.086% Pb and 0.2% others. Strontium carbonate produced from cleaned celestite ore by the method of double decomposition contained iron below 0.10 g/L and calcium below 0.2%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.