Abstract

Ceramic materials with high strength and chemical inertness are widely used as engineering materials. However, the brittle nature limits their applications as fracture occurs before the onset of plastic yielding. There has been limited success despite extensive efforts to enhance the deformability of ceramics. Here we report a method for enhancing the room temperature plastic deformability of ceramics by artificially introducing abundant defects into the materials via preloading at elevated temperatures. After the preloading treatment, single crystal (SC) TiO2 exhibited a substantial increase in deformability, achieving 10% strain at room temperature. SC α-Al2O3 also showed plastic deformability, 6 to 7.5% strain, by using the preloading strategy. These preinjected defects enabled the plastic deformation process of the ceramics at room temperature. These findings suggest a great potential for defect engineering in achieving plasticity in ceramics at room temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.