Abstract

Cr3+-doped Sr3Ga2Ge4O14:0.03Cr3+ (SGGO:0.03Cr3+) phosphor was synthesized via a high-temperature solid-phase method. Considering the tunable structure of SGGO, Ga3+ ions in the matrix were substituted with In3+ ions at a certain concentration. The tuned phosphor produced a red-shifted emission spectrum, with its luminescence intensity at 423 K maintained at 63% of that at room temperature; moreover, the internal quantum efficiency increased to 65.60%, and the external quantum efficiency correspondingly increased to 21.94%. On this basis, SGIGO:0.03Cr3+ was encapsulated into a pc-LED, which was applied in non-destructive testing (NDT) experiments, successfully realizing the recognition of water and anhydrous ethanol, proving its potential application in the field of NDT.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.