Three-millimeter-thick 17vol%SiCp/2009Al-T4 plates were successfully friction stir welded. The ultimate tensile strength of the joints increased as the welding speed increased from 50 to 800mm/min and reached 97% of the base material at 800mm/min, with the fracture location shifting from the first low-hardness zone adjacent to the nugget zone to the nugget zone.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.