Abstract

The influence of the brand of the material from which the magnetic conductors are made on the power characteristics of the magnetic system and magnetic coupling with highly coercive permanent magnets Nd–Fe–B with a residual magnetic induction of 1.1 T is considered. The material of the magnetic conductors is steel 15 or corrosion-resistant steel 08Х22H6T. On average, in the range of air gaps between sections of the magnetic system from 4 to 10 mm, the decrease in the specific shear force with magnetic conductors made of corrosion-resistant steel 08Х22Н6T, relative to magnetic conductors made of steel 15 is 18.15 %.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.