Abstract

The codeposits on JT-60 tiles experienced hydrogen plasma burning were irradiated by focused beams of an excimer laser. The removal rate of the JT-60 codeposits was low when the laser energy density was smaller than the ablation threshold (1.0 J/cm 2), but reached to 1.1 μm/pulse at the laser energy density of 7.6 J/cm 2. The effective absorption coefficient k in the JT-60 codeposits at ArF excimer laser wavelength was determined to be 1.9 μm −1, which is almost one order smaller than the optical absorption coefficient at the same wavelength in graphite (16.4 μm −1). In the process of ablative removal of the codeposits, hydrogen was released predominantly in the form of hydrogen molecule and water formation could be ruled out. The temperature rise on the surface was measured on the basis of Planck’s law of radiation, and the temperature during the irradiation at the laser energy density of 0.5 J/cm 2 decreased from 3570 K at the beginning of the irradiation to 2550 K at 1000th pulse of the irradiation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.