Abstract

To improve the long-term service of existing laminated ceramics at ultra-high temperature, laminated ZrB2-SiC/SiCw (ZSS) ceramic was prepared by hot-pressing with SiCw (SiC-whisker) as interface layer. After ablated in oxyacetylene at 3000 °C for 100 s, the structure of ZSS remained intact and the linear and mass ablation rates were 0.12 ± 0.03 μm s−1 and 0.43 ± 0.09 mg s−1, respectively. Such excellent ablation resistance of ZSS was attributed to the reduction of the surface temperature and the formation of SiO2 layer by SiC whisker, which resulted in prominent oxidation protection and strong bonding strength at interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.