Abstract
The inside of the molding die fabricated by additive manufacturing can locate cooling channels efficiently. However, the internal face of cooling channels has the problem that face roughness of the cooling channels is not uniform due to the partially melted powder. In this research, the method of finishing the internal face by free abrasive grain is proposed. As a result, the internal face roughness in the cooling channel was improved significantly by the removal of the partially melted powder. The cooling channel of smaller diameter has high processability due to the high velocity of flow by passing through the channel.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Proceedings of International Conference on Leading Edge Manufacturing in 21st century : LEM21
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.