Chitosan-silver (CS-Ag) nanocomposite was green synthesised without the aid of any external chemical-reducing agents. The synthesised nanocomposite was characterised by UV–visible spectroscopy, X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermo-gravimetric analysis (TGA), differential scanning calorimetry (DSC), field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDX), atomic force microscopy (AFM), high-resolution transmission electron microscopy (HR-TEM) with selected area electron diffraction (SAED), X-ray photoelectron spectroscopy (XPS), and zeta potential analyser. The particle size of the synthesised CS-Ag nanocomposite was around 20nm and was found to be thermally stable in comparison with pure chitosan. The prepared nanocomposite acts as a photocatalyst for dye decolourisation, with a maximum of 81% of methyl orange (MO) decolourisation that occurred under visible light irradiation. The kinetics was found to follow pseudo-first-order according to Langmuir–Hinshelwood (L–H) model. The nanocomposite also proved to be an excellent antimicrobial agent against both Gram-positive and Gram-negative bacteria, possessing a broad spectrum of antimicrobial activity. The zone of inhibition ranged between 16.000±1.000 and 19.333±1.155 (mm), proving its high susceptibility than chitosan itself. The minimum inhibitory concentration (MIC) values were from 8 to 64μg/mL, whereas the minimum bactericidal concentration (MBC) values ranged from 16 to 128μg/mL, with the highest antibacterial activity shown against Gram-positive Staphlococcus aureus. This report illustrates the eco-friendly approach for the reduction of silver using chitosan as a reducing agent, and its potential to dye decay and microbial contaminants.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call