Abstract

A two-stage pretreatment process is constructed to test the feasibility of lignin-first biomass pretreatment. It is expected that mild pretreatment conditions help to reduce structural alterations to lignin or minimize condensation reactions in lignin which are important for certain high value applications. The pretreatment process consists of a step using 1% sodium hydroxide solution to increase the porosity of biomass and a second step using a typical ionic liquid, 1-ethy-3-methylimidazolium acetate ([C2C1Im][OAc]), to transform native crystalline cellulose into amorphous cellulose and therefore enhance enzymatic hydrolysis efficiency. Both pretreatments are carried out at 60 °C for 3 h to lower the severity of the pretreatment. Lignin samples extracted from untreated biomass (Lignin 1), liquid phase after NaOH pretreatment (lignin 2), liquid phase after subsequent IL pretreatment (lignin 3) and the lignin remaining in pretreated biomass (lignin 4) were analyzed using FTIR and by measuring molecular weight and antioxidant properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.