Abstract

Improving the mechanical properties of Mg alloys is of great significance for their wide application. A micro-alloyed Mg-1.45Bi-0.79Ca alloy (in wt.%) exhibiting a high tensile yield strength of 394 ± 5 MPa and a moderate elongation of 6.6 ± 0.6% was fabricated by single pass extrusion. The superior high strength is mainly attributed to the synergy effects of ultra-fine dynamic recrystallized grains; numerous Mg2Ca, Mg3Bi2, and Mg2Bi2Ca nano-precipitates; residual dislocations; sub-grain boundaries; as well as strong <10-10> fibre texture in the extrusion direction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.