Pechini polymeric precursor method was successfully used to synthesize (Ba 0.95Ca 0.05)(Ti 0.85Zr 0.15)O 3 nano powders. The results of TG/DTA, XRD and IR analyses showed that by heating the precursor between 490 °C and 580 °C, an intermediate phase with possible composition of (Ba,Ca) 2(Ti,Zr) 2O 5CO 3 was formed. Between 580 °C and 700 °C, the intermediate phase transformed to a crystalline solid solution by de-carbonation reaction. The transformation completed at 700 °C. Nano-sized powders with equivalent sphere diameters about 72 nm were obtained by calcination of the precursor at 700 °C for 4 h. The ceramics sintered at 1300 °C for 2 h can reach about 95% theoretical density and the peak dielectric constant is 15,000 at 70 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.