Abstract

To evaluate the dentin and enamel bonding strength and resin-dentin interfaces of four resin cements. Twenty-four sound freshly extracted molars were sectioned with low-speed saw under running water. Two mesial-distal enamel disc and two buccal-lingual dentin discs were sectioned from each molar. Four resin cements (A group: Panavia(TM) F; B group: RelyX(TM) ARC; C group: RelyX(TM) Unicem; D group: Clearfil(TM) SA Cement) were applied to the surface of these enamel and dentin discs according to manufacturers' guidance. The bonded specimen were prepared for shear bond strength test and sectioned occluso-gingivally into two slabs for scanning electron microscopy (SEM) observation. The bonding strength between resin and enamel in B group [(29.38 ± 6.28) MPa] was higher than that in D group [(27.25 ± 7.03) MPa], and both of them were significantly higher than those in A [(22.92 ± 7.13) MPa] and C group [(10.92 ± 3.41) MPa] (P < 0.05). The highest dentin bonding strength was shown in B group [(27.28 ± 6.79) MPa], followed by A [(14.23 ± 6.39) MPa], D [(10.09 ± 3.26) MPa] and C group [(6.43 ± 1.60) MPa, P < 0.05]. The four resin cements have different enamel or dentin bonding properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call