Abstract

This paper presents the mechanical properties and SEM studies of bone cements reinforced by bovine hydroxyapatite (BHA), synthetic hydroxyapatite (HA), and β-tricalcium phosphate (β-TCP). All ceramic fillers were silane treated with γ-methacryloxy-propyl-trimethoxy silane (A-174, 0.2%). The quantities of silane treated ceramic fillers in cement were 1.5 wt.%, 2.5 wt.% and 3.5 wt.%. Commercial CMW™3 bone cement was used as control group. The results showed that there is no decay of mechanical properties if the amount of bioceramic additives does not exceed 2.5 wt.%. Similar microstructures were observed by SEM at the fracture surfaces of the bioceramic reinforced bone cements and the control group.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.