The formation and removal of the carbonaceous deposits formed by n-butane and liquid hydrocarbons, such as n-decane and proprietary light and heavy naphthas, between 973 and 1073 K on YSZ and ceria–YSZ, has been studied to determine conditions for stable operation of direct-utilization SOFC. First, it is shown that deactivation of SOFC with Cu–ceria–YSZ anodes operating on undiluted n-decane, a mixture of 80% n-decane and 20% toluene, or light naphtha at temperatures above 973 K is due to filling of the pores with polyaromatic compounds formed by gas-phase, free-radical reactions. Formation of these compounds occurs at a negligible rate below 973 K but increases rapidly above this temperature. The rate of formation also depends on the residence time of the fuel in the anode compartment. Because steam does not participate in the gas-phase reactions, carbonaceous deposits could form even at a H 2O:C ratio of 1.5, a value greater than the stability threshold predicted by thermodynamic calculations. Temperature programmed oxidation (TPO) measurements with 20% H 2O in He demonstrated that carbon deposits formed in pure YSZ were unreactive below 1073 K, while deposits formed on ceria-YSZ could be removed at temperatures as low as 923 K. Based on these results, we discuss strategies for avoiding carbon formation during the operation of direct-utilization anodes on oil-based liquid fuels.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call