Abstract
The pre-peak loading stages of rock in compression tests are divided into four stages (i.e., crack closure, elastic deformation, stable crack growth and unstable crack growth) by identifying the Crack Closure stress (CC), Crack Initiation stress (CI), and crack damage stress. A new method for determining the CC and CI is presented in this paper and compared with previous methods. The new method is called “Continuous Strain Deviation” (CSD), and it solves two problems associated with other methods: 1) determining the limits for the elastic range in laboratory data, and 2) identifying where crack closure or initiation occurs from the subtle changes in the stress-strain data. Starting from an initial point corresponding to 30% to 40% UCS, the proposed algorithm provides a distinct indicator for CC and CI. The CC and CI for Badaling granite and Äspö diorite are determined with the proposed method, results from which are similar to other methods. Sensitivity analyses of the CSD method show that stable CC and CI values could be estimated using any initial point from 30% to 40% UCS. Comparison studies show that the CSD method predicts a smaller stress range and gives a more distinct indicator for both CC and CI.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.