Abstract

The effect of Zinc-Oxide (ZnO) thin film annealed in different ambiences is presented. To achieve low cost and environmentally friendly process, ZnO aqueous solution is synthesized by dissolving zinc acetate dihydrate in deionized water directly. Zinc oxide aqueous solution of high solubility and stability is presented. High quality and dense Zinc oxide thin film is formed by spin coating. Annealing temperatures are in the range of 300 °C~500 °C, and annealing ambiences of both air and N2 are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.