The novolac-based resins used as positive-tone photoresists are frequently etched in an oxygen plasma. It is desirable to have a predictive model of the photoresist etch rate but, for process improvement, control, and analysis, the development of a rigorous mechanistic model is impractical. Instead, a simplified mechanistic model is derived, here, according to the method proposed by Hougen and Watson for the study of fluid–solid interactions. This model derivation method is employed in order to arrive at a functional form that represents chemical etching of the resist by oxygen radicals, assisted by the plasma ion flux. Values for model parameters are determined from process data by nonlinear regression. The quality of the model fit to the data is tested statistically.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.